性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 4.0 | g/10min | ||
密度 | 23℃ | ASTM D-1505 | 0.923 | g/cm3 | ||
机械性能 | 断裂伸长率 | MD | ASTM D-882 | 18 | MPa | |
TD | ASTM D-882 | 15 | MPa | |||
应力拉伸强度 | MD | ASTM D-882 | 15 | MPa | ||
TD | ASTM D-882 | 11 | MPa |
|
|
性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | 数据单位 | ||
基本性能 | 熔体流动速率 | ASTM D-1238 | 4.0 | g/10min | ||
密度 | 23℃ | ASTM D-1505 | 0.923 | g/cm3 | ||
机械性能 | 断裂伸长率 | MD | ASTM D-882 | 18 | MPa | |
TD | ASTM D-882 | 15 | MPa | |||
应力拉伸强度 | MD | ASTM D-882 | 15 | MPa | ||
TD | ASTM D-882 | 11 | MPa |